To make this part functional
Please print the nozzle with TPU
-0.4mm nozzle
-Concentric Top pattern
-Concentric Bottom pattern
-100% infill Concentric (for rigidity)
-No horizontal expansion changes
Please print the clip with PLA
-0.4mm nozzle
-Cocentric Top & Bottom pattern
-Cocentric 100% infil (rigidity for angular bending)
( Calibrate Tolerance before printing ) Important!
This part is print in place, and the hinge bends.
Please use razor to cut bottom layer after printing to not break the hinge.
Edit model in Fusion360 if needed to adjust for tolerance or use
-Hole horizontal expansion adjustment
Enjoy!