This is a remix of JHB's Articulated Bender. I was always having issues with the tabs inside the articulated parts breaking so I reinforced them.
Material: PLA
Temps: 200C and 60C
Layer Height: 0.16, alternate walls
Layer Width: 0.4
Infill: 50% Gyroid, connect infill
Supports and raft adhesion
6/9: I have discovered that a TINY drop of Super Lube in the areas that move or may be a tighter fit helps out immensely. I’d maybe try a lubricant designed for plastics, but for me it’s working great