V2 Changes:
The neck is now full width to make it stiffer and less likely to "bend" with high speed builds.
The Fin is slightly adjusted for better compatibility with certain sector gears
Ideal print profile:
0.2 Nozzle
0.08 Layer height
50 Walls (or 100% Infill concentric pattern)
Common print profile:
0.4 Nozzle
0.08 Layer height
50 Walls (or 100% Infill concentric pattern)
0.45 Line width.
Refer to the images for ideal print orientation.
Materials:
Tested with
eSun PLA+
Elegoo PLA+.
ABS/ASA, PC or PA should also work.
PETG will 90% break, stock (non-plus) PLA will 100% break. I highly not recommend either of them.