[Update 24.12.01: Applying pressure in two stages can effectively avoid defects caused by material shrinkage. This approach allows for more precise control of the overflow length at the top surface, reducing the time needed for post-process polishing. Initially, 8.8g of PLA was recommended; now, 8.5~8.6g of PLA is advised. After the molten plastic is placed into the mold, apply pressure for 15 seconds, let it sit for 1 minute, and then apply pressure again for another 15 seconds.]